WEKO3
アイテム
超音波加振型加圧焼結法によるNi,Ti,NiTi各金属/グラフェン複合焼結体の作製と特性評価
https://nagano-nct.repo.nii.ac.jp/records/2000078
https://nagano-nct.repo.nii.ac.jp/records/2000078edefe00d-619b-4e70-91fb-7c23111f81b2
| 名前 / ファイル | ライセンス | アクション |
|---|---|---|
|
|
|
| アイテムタイプ | 教育研究報告 / Departmental Bulletin Paper(1) | |||||||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 公開日 | 2024-08-30 | |||||||||||||||||
| タイトル | ||||||||||||||||||
| タイトル | 超音波加振型加圧焼結法によるNi,Ti,NiTi各金属/グラフェン複合焼結体の作製と特性評価 | |||||||||||||||||
| 言語 | ja | |||||||||||||||||
| タイトル | ||||||||||||||||||
| タイトル | Manufacture and property of each Ni, Ti, NiTi metal/graphene composite by ultrasonic-assisted hot-pressing method | |||||||||||||||||
| 言語 | en | |||||||||||||||||
| 言語 | ||||||||||||||||||
| 言語 | jpn | |||||||||||||||||
| キーワード | ||||||||||||||||||
| 言語 | ja | |||||||||||||||||
| 主題Scheme | Other | |||||||||||||||||
| 主題 | グラフェン | |||||||||||||||||
| キーワード | ||||||||||||||||||
| 言語 | en | |||||||||||||||||
| 主題Scheme | Other | |||||||||||||||||
| 主題 | Ni | |||||||||||||||||
| キーワード | ||||||||||||||||||
| 言語 | en | |||||||||||||||||
| 主題Scheme | Other | |||||||||||||||||
| 主題 | Ti | |||||||||||||||||
| キーワード | ||||||||||||||||||
| 言語 | en | |||||||||||||||||
| 主題Scheme | Other | |||||||||||||||||
| 主題 | NiTi | |||||||||||||||||
| キーワード | ||||||||||||||||||
| 言語 | ja | |||||||||||||||||
| 主題Scheme | Other | |||||||||||||||||
| 主題 | ホットプレス法 | |||||||||||||||||
| 資源タイプ | ||||||||||||||||||
| 資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||||||||||||||
| 資源タイプ | departmental bulletin paper | |||||||||||||||||
| 著者 |
堀口勝三
× 堀口勝三
× 森山実
× 押田京一
|
|||||||||||||||||
| 抄録 | ||||||||||||||||||
| 内容記述タイプ | Abstract | |||||||||||||||||
| 内容記述 | The composites containing 0% or 15 vol% of graphene (GnP) for each matrix metal of Ni, Ti and NiTi were prepared by hot pressing method with or without assistance of ultra-sonic waves, and the mechanical and electrical properties were compared. The relative density of Ni and Ti-based metals with 0% GnP content was 96% or higher. When 15 vol% GnP was included, it decreased to about 84-94%. The relative density of the NiTi with 0% GnP content increased from 90.6% to 98.2% by applying ultrasonics. However, when GnP was included, it decreased to 91.1-92.4%. The mechanical properties showed proportional to the relative density. The electrical conductivities of pure Ni, Ti, and NiTi metals were 9.09, 1.78 and 1.19 MS/m, respectively. The electrical conductivity of composite with 15vol% of GnP decreased, particularly for Ni-based and Ti-based materials, which decreased to 22-53%. |
|||||||||||||||||
| 言語 | en | |||||||||||||||||
| 書誌情報 |
巻 1, 号 2-09, 発行日 2024-08-30 |
|||||||||||||||||
| 出版者 | ||||||||||||||||||
| 出版者 | 長野工業高等専門学校 | |||||||||||||||||
| 言語 | ja | |||||||||||||||||
| ISSN | ||||||||||||||||||
| 収録物識別子タイプ | ISSN | |||||||||||||||||
| 収録物識別子 | 1882-9155 | |||||||||||||||||
| 書誌レコードID | ||||||||||||||||||
| 収録物識別子タイプ | NCID | |||||||||||||||||
| 収録物識別子 | AA1259397X | |||||||||||||||||
| 見出し | ||||||||||||||||||
| 大見出し | 研究報告 | |||||||||||||||||
| 言語 | ja | |||||||||||||||||